Cupro B2 CuBe2 UBE2

 

Chemical
Composition

Be Co+Ni Others Cu
2.00 0.50 0.50 maks. Remaining

 

 

 

Code : DIN 17672 – W. Nr. 2. 1247, EN: 101C, AFNOR: Ube2, USA CDA: C17200, RWMA: Class 4

Cupro B2 Material Properties: Hardness is the highest copper alloy. 40 - 41 RC is reached. Optionally, case hardened or solution obtained condition (20 - 22 RC) will be delivered.

Cupro B2 Areas of Application:
•Flash welding dies, rim and chain welding
•In the plastic moulds as chill plates and inserts in the moulds, cooling pins and neck rings or bottom plates for blow moulds of plastic bottles

•Parts for electrical components
•Safety tools due to non-sparking, non-magnetic and corrosion resistant features.

Heat Treatment at 370 – 450 °C, between 2 oto 4 times

Mechanical Properties:

Hardness HB 340-390
Tensile Strength N/mm² 1100-1300
Yield Strength N/mm² 1000
Elongation L=5D % 4-5
Modulus of Elasticity (20 °C)  kN/mm2 128
 

Physical Properties :

Electrical Conductivity % 22
Coefficient of Thermal Expansion 1/K 17.5•10-6
Thermal Conductivity (20 °C) N/mm² 106
Intensity % 8.3