1.8550 (34CrAINi7) steel is designed to be used in applications requiring high corrosion, temperature, wear, and fatigue resistance. It is a nitriding steel commonly alloyed with chromium, aluminum, nitrate, and molybdenum, which allows for achieving a surface hardness of at least 950 HV after nitriding. It is widely used in energy, machinery, and automotive industries when in the heat-treated condition.
Carbon |
Chromium |
Molybdenum |
Nickel |
Aluminum |
C |
Cr |
Mo |
Ni |
Al |
0,34 |
1,70 |
0,20 |
1,00 |
1,00 |
|
Temperature |
Cooling |
Hardness |
Soft annealing |
650 - 700°C |
furnace |
|
Normalizing |
860 - 900°C |
furnace |
|
Hardening |
870 - 930°C |
oil, pressure gas (N2), air or hot bath 500 - 550°C |
See Tempering Diagram |
Hardness |
27 - 33 |
HRC |
Tensile strength |
800 - 1100 |
N/mm2 |
Yield strength |
600 - 680 |
kN/mm2 |
ElongationL=5D |
10 - 13 |
% |
Toughness |
30 - 35 |
CVN (J) |
Coefficient of thermal expansion |
12,1 - 13,7 |
1/K * 10-6 |
Thermal conductivity (20°C)
|
33,7 |
W/mK |
Density |
7,80 |
g/cm3 |
We use cookies that comply with legal regulations to improve your shopping experience. You can find detailed information on our Cookie Policy page